Q345 steel plate

Dec 11, 2025 Læg en besked

Q345 series steel includes Q345A, Q345B, Q345C, Q345D, and Q345E, where Q represents the yield strength, the latter number 345 represents the yield point value (in MPa), and the letters A, B, C, D, and E respectively represent the low-temperature impact resistance of the steel, mainly due to the different impact temperatures. In short, Q345A does not do impact;Q345B, 20 ℃ room temperature impact;Q345C, 0℃impact; Q345D, -20℃impact;Q345E, -40 impact. Different impact temperature, impact value is also different.

 

Yield Strength: Min 345 MPa (for thickness <= 16mm).

Tensile Strength: 470-630 MPa.

Grades: A, B, C, D, E (varying impact tests).

Features: Excellent weldability, good formability, toughness.

Q345A: Basic grade, no specific impact testing.

Q345B: Impact test at 0℃ (34 J).

Q345C: Impact test at 0℃ (34 J).

Q345D: Impact test at -20℃ (34 J).

Q345E: Impact test at -40℃ (27 J).

 

 

CHEMICAL COMPOSITION OF Q345 SERIES STEEL

 

C

P

S

V

Q345A

0.12-0.2

0.20-0.6

1.00-1.6

<=0.045

<=0.045

<=0.3

<=0.3

<=0.2

0.02-0.15

Q345B

0.12-0.2

0.20-0.6

1.00-1.6

<=0.04

<=0.04

<=0.3

<=0.3

<=0.2

0.02-0.15

Q345C

0.12-0.2

0.20-0.6

1.00-1.6

<=0.035

<=0.035

<=0.3

<=0.3

<=0.2

0.02-0.15

Q345D

<=0.18

0.20-0.6

1.00-1.6

<=0.03

<=0.03

<=0.3

<=0.3

<=0.2

0.02-0.15

Q345E

<=0.18

0.20-0.6

1.00-1.6

<=0.025

<=0.025

<=0.3

<=0.3

<=0.2

0.02-0.15

 

MECHANICAL PROPERTY OF Q345 SERIES STEEL

 

Q345A

490-675

>=345

>=21

Q345B

490-675

>=345

>=21

Q345C

490-675

>=345

>=22

Q345D

490-675

>=345

>=22

Q345E

490-675

>=345

>=22