ASTM A302 steel plate

Dec 05, 2025 Læg en besked

ASTM A302 is a kind of low alloy steel specification covers 4 different grades(A, B, C, D), Grade C and D contains chemical composition Ni, with the same thickness, yield and tensile strength of Grade C is the same of Grade B, while elongation rate of grade C is higher.

This specification covers manganese-molybdenum and manganese-molybdenum-nickel alloy steel plates intended particularly for welded boilers and other pressure vessels. ASTM A302 is a kind of low alloy steel specification covers 4 different grades(A, B, C, D), Grade C and D contains chemical composition Ni, with the same thickness, yield and tensile strength of Grade C is the same of Grade B, while elongation rate of grade C is higher. It is manufactured for Pressure Vessel, Boiler, Storage Tanks and Heat Exchanger in Oil, Gas Project.

 

Thickness: 6mm-300mm

Length: 3000mm-15000mm

Width: 1500mm-4050mm

 

Supplementary Technology: UT, AR, TMCP, N, Q+T, Z Direction Test(Z15,Z25,Z35), Charpy V-Notch Impact Test, HIC test, NDT ,PWHT( Simulated Post Weld Heat Treatment), NACE0175, The Third Party Test (Such as SGS Test).

 

ASTM A302 Chemical Composition

ASTM A302 Chemical Composition
C P S
A302 Grade A 0.20-0.25 0.13–0.45 0.87–1.41 0,035 0,035 0.41–0.64  
A302 Grade B 0.20-0.25 0.13-0.45 1.07-1.62 0.035 0.035 0.41-0.64  
A302 Grade C 0.20-0.25 0.13-0.45 1.07-1.62 0.035 0.035 0.41-0.64 0.37-0.73
A302 Grade D 0.20-0.25 0.13-0.45 1.07-1.62 0.035 0.035 0.41-0.64 0.67-1.03

 

ASTM A302 Mechanical Property:

  ASTM A302 Mechanical Property
A302 Grade A
6-50 310 515-655 19%
50-200 310 515-655 15%
A302 Grade B 6-50 345 Mpa 550-690 Mpa 18%
50-200 345 Mpa 550-690 Mpa 15%
A302 Grade C 6-50 50 [345] 80-100kis [550-690]Mpa 17%
50-200 20%

 

ASTM A302 Equivalent steel grade:

U.K.
ASTM A302 Gr. A,B 14Cr Mo 45 13 Cr Mo 44 15 CD 4.05 14 Cr Mo 46 620 Gr.27,31